Products

Carbon fibre prepreg

Reinforcement pre-impregnated with resin at the mill at a controlled resin content, supplied interleaved with release paper and polyethylene film. Chosen where repeatable fibre volume and consistent mechanical performance matter more than the flexibility of wet layup.

Specification

PropertyTypical value
ReinforcementCarbon, E-glass, S-glass and aramid
ConstructionUnidirectional and woven
MatrixEpoxy, low and elevated temperature cure systems
FormatInterleaved with release paper and polyethylene film
StorageFrozen storage required, shelf life and out-life confirmed per order
Cure scheduleMatched to the equipment you have

What prepreg is

Prepreg is reinforcement that has already been impregnated with a resin system at the mill, at a controlled resin content, then partially advanced so it is tacky rather than wet. You lay it up, apply heat and usually pressure, and the resin completes its cure.

The appeal is control. In wet layup the resin content varies with the person holding the roller, so two parts off the same mould are never quite the same. In prepreg the fibre to resin ratio is set before the material reaches you, which is why aerospace and motorsport structures are built from it and why anyone chasing repeatable performance eventually moves to it.

The cost is logistics. The advanced resin keeps advancing, slowly, whenever the material sits above freezing, so prepreg carries two clocks: a shelf life at frozen storage, and an out-life at room temperature that accumulates every time the roll comes out. Neither resets.

Carbon, E-glass, S-glass and aramid

Carbon prepreg is the stiffness choice, and the lightest for an equivalent structural job. It is the default for UAV airframes, tubes, motorsport components and anything where deflection under load is the binding constraint. It conducts electricity, which matters when a part sits near antennas or sensors.

Glass prepreg costs less, weighs more for the same structural job, and does not conduct electricity or interfere with radio signals. That last property is why it is chosen far more often than people assume: radomes, antenna housings and electrical enclosures are glass rather than carbon regardless of budget.

Glass prepreg comes in two grades. E-glass is the general purpose grade and covers most insulating and signal transparent work. S-glass is the higher strength grade relative to E-glass, used in defence, aerospace and radome work where strength and impact performance matter, and it keeps the electrical insulation and signal transparency that make glass the choice in the first place.

Aramid prepreg is the toughness choice. It absorbs impact energy and resists abrasion where carbon fractures, and it tends to deform rather than shatter when overloaded. It is difficult to cut and machine cleanly and it takes up moisture more readily than the other two, both of which want planning for at design stage rather than discovering on the bench.

Hybrid layups are common and sensible: carbon for the structural plies with aramid on the impact face, or a glass ply at the surface where an electrical break is needed.

Matching material to the equipment you have

The most common specification failure we see is a resin system that the customer cannot cure. There is no point ordering a material that needs an elevated temperature cure if your oven cannot reach and hold it, and no point planning around an autoclave you do not have.

Four things decide whether a given prepreg fits your shop. Whether you have frozen storage, and how much. How long the material will sit at room temperature across the whole layup, because out-life accumulates. What temperature and dwell your oven or autoclave can actually hold. And whether your tooling will survive the cure, which rules some tooling materials out.

If those four do not line up, the fibre choice is academic and dry fabric with a wet layup is the better route. We would rather tell you that than sell you material you cannot process.

Glass transition temperature is the other number worth understanding before you compare datasheets, because it is measured three different ways and the figures are not interchangeable. The guides below cover it in full.

What to send us when you ask for a quote

Reinforcement type and format first: carbon, E-glass, S-glass or aramid, and unidirectional or woven. If woven, which weave, because two fabrics at the same areal weight behave differently over a tight radius.

Then areal weight in gsm rather than a target thickness, since areal weight is what the mill produces to and thickness follows from it. Then the resin content if you have a figure you tested with, because otherwise you will get the house standard.

Then the cure schedule you can actually run, stated as the temperature and dwell your equipment holds, and the service temperature the finished part has to survive. Those two together let us work backward to a resin system rather than guessing.

Finally the roll width that suits your part, since width drives how much you trim off every ply, and the quantity. Documentation requirements are agreed at quotation stage, so raise them with the enquiry.

Resin system, cure schedule, areal weight and roll width are confirmed against your application at quotation stage.

Where it is used

  • Tubes and profiles

    Rolled or moulded over a mandrel, where fibre angles need varying through the wall.

  • UAV and airframe components

    Structure that has to come off the tool the same every time, batch after batch.

  • Sporting goods

    Parts where repeatable stiffness is the product, and a hand layup will not hold it.

  • Industrial and structural components

    Components whose fibre volume is specified rather than left to whoever holds the roller.

  • Radomes and electrical enclosures in glass

    Glass prepreg here rather than carbon, because the part must not interfere with a signal.

Common questions

What is the difference between prepreg and dry fabric?

Prepreg arrives already impregnated with resin at a controlled content set at the mill, which gives repeatable fibre to resin ratios from part to part. Dry fabric has no resin in it and you add it during layup or infusion. Prepreg is more consistent, dry fabric is more flexible and needs no freezer or oven.

Do I need a freezer to store prepreg?

Yes. Prepreg is stored frozen, and the shelf life quoted on any datasheet assumes that. Without frozen storage your usable window is the out-life alone, which is much shorter, so confirm your storage before ordering rather than after.

What is out-life and why does it matter?

Out-life is the total time the material can spend at room temperature before the resin has advanced too far to process. It accumulates: a roll taken out four times for two hours has used eight hours of it, and nothing resets that. Plan the layup around it and keep a log.

Do I need an autoclave?

Not always. Some systems are formulated to cure in an oven under vacuum pressure alone, others need autoclave pressure to reach their stated properties. Tell us what equipment you have and we will match a system to it rather than assuming.

Can I get a resin system that cures at a lower temperature?

Usually yes. Low temperature curing systems exist and are formulated to reach a glass transition temperature above their own cure temperature. State the temperature and dwell your oven can hold and the service temperature the part sees, and we will work backward to a system that fits both.

Do you supply glass and aramid prepreg as well as carbon?

Yes. Carbon, E-glass, S-glass and aramid prepreg are all supplied. Glass is chosen where electrical insulation or signal transparency is required, aramid where impact and abrasion resistance matter more than stiffness, and hybrid layups combining them are common.

What is the difference between E-glass and S-glass prepreg?

E-glass is the general purpose glass grade and the usual choice for insulating and signal transparent parts. S-glass is the higher strength grade relative to E-glass, used in defence, aerospace and radome work where strength and impact performance matter. Both keep the electrical insulation and signal transparency of glass, so the choice comes down to how much strength the part needs and what the budget allows.

Related materials

Further reading

Cure schedule first

There is no point specifying a resin that cures at 120 degrees if your oven reaches 90. Tell us the cure equipment you have and the service temperature the part sees, and we will work backward to a system that fits both.